The damage happens at atomic scale, invisible to routine inspection.
Fastener risk comes mainly from the first route. Cathodic coatings such as zinc and nickel plating generate hydrogen during deposition, and thread roots and head fillets are stress concentrations where hydrogen accumulates.
That explains a familiar pattern: identical process, yet low class bolts run for years while high class ones fracture soon after assembly. The process did not suddenly degrade; the material tolerance for hydrogen fell.
Together these point strongly to hydrogen embrittlement, though stress corrosion cracking and overload should be excluded: the first needs a corrosive medium, the second leaves a visible plastic zone.
A third route is material change. Austenitic stainless is far less sensitive to hydrogen than high strength carbon and alloy steel, so it removes the problem entirely where risk is high.
Geometry can also relieve it. The thread to shank fillet, head bearing face and thread runout all affect local stress. Drawings often simplify these details, yet they influence sensitivity noticeably.
A delayed fracture test applies sustained load and observes for a defined period. The cycle is long, so it is run at first article or after process change rather than in routine inspection.
The technical agreement should state hydrogen control requirements: applicable classes, bake parameters and verification method. Export, automotive and rail customers almost always include this clause.
Zhuhai Jiali Hardware (FASTKING) retains records by lot. See the product centre and the online calculator collection.
Zhuhai Jiali Hardware (FASTKING) Tel +86-756-8586520 Mobile 13928071304 Email lizhong@zhjiali.com No.56-301, Mingzhu North Road, Qianshan, Xiangzhou, Zhuhai. Please contact us.